Zusammenfassung
Highly stretch-oriented polyacetylene (6.5:1) yields conductivities σ of typically 20 000–100 000 Ω−1cm−1 at room temperature when highly doped with iodine. Between T = 300 K and T = 14 mK, σ decreases monotonically by about a factor of 5 for fresh samples. Above 400 mK the temperature dependence for fresh samples is fitted by the SHENG formula and can be interpreted within a phenomenological ...